Barium titanate buffer layers were successfully applied to cube textured Ni-tapes fabricated from commercially available nickel by a chemical solution deposition route. Barium acetate solutions in anhydrous acetic acid were mixed with bis(pentane-2,4-dionato)-titanium(IV)-oxide dissolved in methanol. A slight excess of acetic acid anhydride assured the anhydrous medium. The precursor solution was spin-coated to the Ni-substrate. Heat treatment at 1 000°C under a reducing atmosphere (Ar + 6.5 vol-% H_2) resulted in dense c-axis oriented, a-b in-plane aligned buffer layers.
机译:钛酸钡缓冲层已通过化学溶液沉积方法成功地应用于了由市售镍制成的立方织构镍带。将乙酸钡在无水乙酸中的溶液与溶解在甲醇中的双(戊烷-2,4- dionato)-钛(IV)-氧化物混合。稍微过量的乙酸酐确保了无水介质。将前体溶液旋涂到Ni衬底上。在还原气氛(Ar + 6.5 vol%H_2)下于1000°C进行热处理,得到致密的c轴取向,a-b面内对齐的缓冲层。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号