Large-scale fatigue tests have shown that the crack propagation through the chord wall in square hollow section T-joints is very different from those observed in circular hollow section T-joints, especially the fatigue crack surface under the weld toe. This paper details an experimental investigation on the crack surface under the weld toe in four (4) large-scale square hollow section T-joint specimens. The test results revealed that the crack has a twisted crack surface. The crack not only curved under the weld toe but also changed significantly with the crack location around the weld toe. Further numerical investigation is conducted to study the significance of the crack surface on the distributions of the stress intensity factors around the crack front. A general formula is proposed to define the crack surface for fracture mechanics analysis to predict the residual life of cracked square hollow section T-joints.
机译:大规模疲劳试验表明,通过方形中空部分T关节中的弦壁的裂纹传播与圆形中空部分T关节中观察到的那些,特别是焊接脚趾下方的疲劳裂缝表面。本文详述了四(4)个大型方形中空部分T关节标本中焊接脚趾下裂纹表面的实验研究。测试结果表明,裂缝具有扭曲的裂缝表面。裂缝不仅在焊接脚趾下弯曲,而且在焊接脚趾周围的裂缝位置也显着变化。进行了进一步的数值调查,以研究裂缝表面对裂缝前方周围应力强度因子分布的重要性。提出了通式以限定用于断裂力学分析的裂纹表面,以预测裂纹方形中空部分T关节的残余寿命。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号