Creep-rupture of service-exposed base metal and weldments of alloy 800H

机译:暴露在外的贱金属和800H合金焊件的蠕变断裂

获取原文

摘要

An alloy 800H outlet manifold with weldments made using welding Electrode 112 was removed from service after normal operation at approximately 870 deg C for 64,000 hours, because nondestructive testin gindicated cracks in the circumferential butt welds. The objective of the research was to evaluate th remaining creep-life of the manifold, based on creep-rupture testin gof base metal and weld metal specimens. This information was then used to evaluate similar manifolds that had been repaired and left in service. Creep-rupture tests were performed at stress levels comparable to the service stress and temperatures above the design temperature were selected to accelerate the testing. The results showe dthat the base metal did not suffer significant creep damage from the prior service exposure and that the weld metal had a very low resistance to creep damage. Metallographic analysis of a weld sample taken from a comparable in-service manifold supported this conclusion, and data for new material reported in the literature support the finding of low high-temperature creep strength for welds made using welding Electrode 112. It was recommended to replace or refurbish the welds using welding Electrode 117, which has a greater creep strength.
机译:在约870摄氏度下正常运行64,000小时后,使用焊接电极112制成的带有焊接件的合金800H出口歧管被停用,因为在周向对接焊缝中无损检测到裂纹。该研究的目的是基于在基体金属和焊缝金属试样上的蠕变断裂试验来评估歧管的剩余蠕变寿命。然后,该信息将用于评估已修复并投入使用的类似歧管。在与工作应力相当的应力水平下进行了蠕变断裂测试,并选择了高于设计温度的温度以加快测试速度。结果表明,母材不会因先前的使用而遭受明显的蠕变损伤,并且焊缝金属的蠕变损伤电阻非常低。从可比较的在役歧管中获取的焊缝样品的金相分析支持了这一结论,文献中报道的新材料的数据也支持发现使用焊接电极112制成的焊缝具有较低的高温蠕变强度。建议替换该焊缝或使用焊接蠕变强度更高的焊条117翻新焊缝。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号