Modeling and mitigation of stress corrosion cracking in closure welds of high-level waste container for yucca mountain

机译:丝兰山高级废料容器封闭焊缝中应力腐蚀开裂的建模与缓解

获取原文

摘要

EDA II Desifgn Concept. As described in the License Application Design Selection Report, the recommended waste package design is Engineering Design Alternative II (CRWMS M&O 1999). This design includes a double-wall waste package (WP) underneath a protective drip shield (DS). A schematic representation of the WP is shown in Figure 1. The waste package outer barrier (WPOB) is to be made of Alloy 22 (UNS N06022), which the underlying structural support is to be made of 316NG or 316L (UNSS31603)(Treseder et al. 1991). Alloy 22 is a high-performance nickel-based alloy with substantial amounts of chromium (21
机译:EDA II设计概念。如许可证申请设计选择报告中所述,建议的废物包装设计是“工程设计替代方案II”(CRWMS M&O 1999)。这种设计包括在防滴漏罩(DS)下方的双层废物包装(WP)。 WP的示意图如图1所示。废物包装的外部屏障(WPOB)由22号合金(UNS N06022)制成,其底层结构支撑层由316NG或316L(UNSS31603)(Treseder)制成。等(1991)。合金22是一种高性能的镍基合金,其中含有大量的铬(21

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号