The effect of the core/skin ratio on the overall flow behaviour in the co-injection molding process was studied. A 7.6x16.4x0.7 cm~3 rectangular plaque was moulded using a 150-ton Engel co-injection machine. ABS was used both for the skin and core material and PC were used only as the skin material. For visualization purposes, a black pigment was added to the core material. The results are discussed in terms of the relative viscosity, injection speed, melt and mould temperatures.