QUANTIFYING THE EFFECTS OF STRAINING-HARDENING AND WATER CHEMISTRY ON CRACK GROWTH RATES OF 316L SS WELDS IN HIGH TEMPERATURE WATER

机译:量化应变硬化和水化学对高温水316LS焊缝裂纹生长速率的影响

获取原文

摘要

A series of stress corrosion crack (SCC) growth rate tests with in-situ crack length monitoring for 316L stainless steel weld heat-affected zones with different Vickers hardness and 316 weld metals with different delta-ferrite contents in 288°C pure water with different concentrations of dissolved oxygen were performed. Typical intergranular stress corrosion cracking (IGSCC) and branching of the crack front were observed for two 316L HAZ specimens. Crack growth rate increases with Vickers Hardness in the 316L HAZ specimens. CGRs for 316L HAZ specimens in 2ppm and 7ppm DO are moderately higher than that in 0.2ppm DO water. After a single overloading, CGR tends to be lower for a period of time. Crack growth near the fusion line is monitored and the crack front of a 316L HAZ specimen is near the fusion line, while ACPD still shows an increase before stopping the test.
机译:一系列应力腐蚀裂纹(SCC)生长速率试验,对316L不锈钢焊接热影响区域的原位裂缝长度监测,具有不同的维氏硬度和316个焊接金属,在288°C纯水中具有不同的δ-铁氧体含量不同进行溶解氧的浓度。为两个316L HAZ标本观察到典型的晶间应力腐蚀裂解(IGSCC)和裂缝前面的分支。在316L HAZ标本中,裂纹增长率随着Vickers硬度增加。 316L HAZ标本中的CGR在2ppm和7ppm中的确实比0.2ppm在0.2ppm中的水平高于0.2ppm。在单个过载后,CGR趋于较低一段时间。监测融合线附近的裂缝增长,316L HAZ标本的裂缝前方近融合线,而ACPD仍在停止测试之前显示出增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号