ATMOSPHERIC LEACHING OF ZINC SULPHIDE CONCENTRATES USING REGENERATED FERRIC SULPHATE SOLUTIONS

机译:再生硫酸铁溶液对硫化锌精矿的大气浸出

获取原文
获取原文并翻译 | 示例

摘要

Most of the world's zinc metal is produced via the roast- leach-electrowinning (RLE) process. The process is well established, but most of the sulphur in the sphalerite concentrates reports in the acid, which has to be stored and/or sold. There are significant incentives to develop a simpler process with much reduced acid generation. Ferric ion is a well known oxidant for most sulphides, in particular sphalerite, and it converts the sulphide to elemental sulphur. Based on stoichiometry, however, the amount of ferric ion needed to achieve acceptable zinc extractions is prohibitive for downstream zinc recovery from the leach solutions. The process suggested here makes use of less-than-stoichiometric ferric sulphate additions because the ferric ion is regenerated by sparging SO_2/O_2 mixtures. This regeneration can be effected in-situ in the leach vessel or outside the leach vessel. An example of the application of this new process is presented for a Canadian sphalerite concentrate assaying 60% Zn. The effects of temperature, ferric concentration and ferric ion regeneration are presented. Options to recover zinc from the leach solution are also briefly discussed.
机译:世界上大多数锌金属是通过焙烧-电解沉积(RLE)工艺生产的。该方法已经很好地建立了,但是闪锌矿精矿中的大多数硫都以酸报告,必须存储和/或出售。有很大的动机去开发一种减少酸产生的简单方法。铁离子是大多数硫化物,特别是闪锌矿的众所周知的氧化剂,它可以将硫化物转化为元素硫。然而,基于化学计量,实现可接受的锌提取所需的三价铁离子的量对于从浸提溶液中下游锌的回收是禁止的。这里提出的方法使用了少于化学计量的硫酸铁添加剂,因为铁离子是通过喷射SO_2 / O_2混合物而再生的。该再生可在浸出容器中原位进行或在浸出容器外进行。该新方法的应用示例是针对加拿大闪锌矿精矿测定60%Zn的应用。给出了温度,铁浓度和铁离子再生的影响。还简要讨论了从浸出溶液中回收锌的方法。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号