ELECTROMAGNETIC SHIELDING CAPACITY OF NICKEL-LOADED LIGNITE CHAR OBTAINED BY CARBONIZATION AT 900℃

机译:900℃碳渗碳镍负载褐煤焦炭的电磁屏蔽能力

获取原文
获取原文并翻译 | 示例

摘要

Several significant findings obtained through this study are as follows: Among coals tested, BL is the most suitable material for the production of crystallized carbon, probably because of the high quantity of oxygen-containing group. Carbonization at 800℃ is adequate for producing crystallized carbon from BL. BL char obtained at 900℃-carbonization has a practical EMS capacity by nickel loading of 2wt%. In the case of co-loading of nickel and calcium, the optimam co-loading existed in terms of the formation of crystallized carbon and EMS capacity, which is believed due to the promoting effect of calcium.
机译:通过这项研究获得的一些重要发现如下:在所测试的煤中,BL是最适合生产结晶碳的材料,这可能是因为含氧基团数量很高。 800℃的碳化足以从BL中生产结晶碳。在900℃碳化下获得的BL炭具有2wt%的镍载量,具有实际的EMS容量。在镍和钙的共同负载的情况下,就结晶碳的形成和EMS容量而言,存在最佳的共同负载,这被认为是由于钙的促进作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号