CORRELATION OF THERMAL, TENSILE AND CORROSION PARAMETERS OF ZN-AL ALLOYS WITH COLUMNAR, EQUIAXED AND TRANSITION STRUCTURES

机译:ZN-Al合金的热,拉伸和腐蚀参数与立柱,均等和过渡结构的相互关系

获取原文
获取原文并翻译 | 示例

摘要

The columnar to equiaxed transition (CET) has been examined in different wrought and casting alloys for many years and the metallurgical significance of CET has been treated in several articles. Experimental observations in the literature have focused on thermal parameters like cooling rate, velocity of the liquidus and solidus fronts, local solidification time, temperature gradients and recalescence. The objective of the present research consist on studying the influence of solidification thermal parameters on the type of structure (columnar, equiaxial or with the CET) and on the secondary dendritic spacing in Zn-Al alloys (Zn-1%Al and Zn-4wt%Al, weight percent). Also, correlate the thermal and structural parameters of these alloys with tensile and corrosion behavior. The results show that Zn-4wt%Al alloys are more resistant to the corrosion that Zn-lwt%Al, independently of the structure. Also, in both alloys the equiaxed structures presented a better tensile resistance than the columnar and CET zones.
机译:多年以来,已经在不同的锻造和铸造合金中研究了柱状至等轴转变(CET),并且在几篇文章中都论述了CET的冶金学意义。文献中的实验观察集中在热参数上,例如冷却速率,液相线和固相线前沿的速度,局部凝固时间,温度梯度和重新发光。本研究的目的在于研究凝固热参数对结构类型(立柱,等轴或与CET)的影响以及对Zn-Al合金(Zn-1%Al和Zn-4wt)的二次枝晶间距的影响。 (%Al,重量%)。同样,将这些合金的热和结构参数与拉伸和腐蚀行为相关联。结果表明,Zn-4wt%Al合金比Zn-1wt%Al更耐腐蚀,而与结构无关。同样,在两种合金中,等轴结构都比柱状区和CET区具有更好的抗拉伸性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号