A356.2 aluminum alloy is a popular commercial alloy used for structural shaped castings in automotive applications. The heat treatment of this alloy is critical to obtain the desired mechanical and performance properties. The three stages of heat treatment include, solutionizing, quenching and artificial ageing. In this study, the effect of quenching in water at 80 ℃ and forced air at 37.4 ms~(-1) velocity is quantified. Further, the effect of natural ageing treatment prior to the artificial ageing is also quantified. It is observed that the mechanical properties of the castings are significantly affected by both the rate of quenching and the natural ageing treatment. Mechanical properties and hardness values are presented for standard uniaxial tensile test specimen cast by gravity permanent mold process and subjected to various heat treatment conditions.
机译:A356.2铝合金是一种流行的商用合金,用于汽车应用中的结构异型铸件。这种合金的热处理对于获得所需的机械性能和性能至关重要。热处理的三个阶段包括固溶,淬火和人工时效。在本研究中,量化了在80℃的水中淬火和在37.4 ms〜(-1)速度下的强制空气淬火的影响。此外,还可以量化在人工时效之前的自然时效处理的效果。可以看出,淬火速率和自然时效处理都显着影响铸件的机械性能。给出了通过重力永久铸模工艺铸造并经过各种热处理条件的标准单轴拉伸试样的机械性能和硬度值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号