Preparation of Orange-Red Long Afterglow Phosphors Y2O2S: Sm3+ , Mg2+ , Ti4+

机译:橘红色长余辉荧光粉Y2O2S的制备:Sm3 +,Mg2 +,Ti4 +

获取原文
获取原文并翻译 | 示例

摘要

The orange-red long afterglow phosphors Y2O2S:Sm3+, Mg2+, Ti4+ was prepared by high temperature solidstate method. By XRD analysis, the crystal phase of the sample was Y2O2S, belonging to hexagonal system, and no new crystal phase arose when doping Sm3+, Mg2+, Ti4+ . The characteristic peaks of excitation spectrum were located at 373,388,417, 430, 475 and 491 nm, and the characteristic peaks of emission spectrum were located at 571, 609 and 657 nm. The content of Sm3+ and doped ions Mg2+, Ti4 + affected the luminescent properties obviously, and Sm3 + affected the luminescent brightness mainly. Mg2+ and Ti4+ could deepen properly trap energy of Y2O2S crystal and strengthen its afterglow properties, the brightness and afterglow properties of sample were better when the mole ratio of Sm/Y, Mg/Y and Ti/Y is 1.4%, 1.25% and 0.9%, respectively.
机译:采用高温固态法制备了橙红色长余辉荧光粉Y2O2S:Sm3 +,Mg2 +,Ti4 +。通过XRD分析,样品的晶相为Y 2 O 2 S,属于六方晶系,掺杂Sm 3+,Mg 2+,Ti 4+时不出现新的晶相。激发光谱的特征峰位于373,388,417、430、475和491 nm,发射光谱的特征峰位于571、609和657 nm。 Sm3 +和掺杂离子Mg2 +,Ti4 +的含量对发光性能有明显影响,而Sm3 +主要影响发光亮度。 Mg2 +和Ti4 +可以适当地加深Y2O2S晶体的能量并增强其余辉性能,当Sm / Y,Mg / Y和Ti / Y的摩尔比为1.4%,1.25%和0.9时,样品的亮度和余辉性能更好。 %, 分别。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号