【24h】

Air Oxidation Kinetics Study of Zr_(58)Nb_3Cu_(16)Ni_(13)Al_(10) Bulk Metallic Glass

机译:Zr_(58)Nb_3Cu_(16)Ni_(13)Al_(10)大块金属玻璃的空气氧化动力学研究

获取原文
获取原文并翻译 | 示例

摘要

The isothermal oxidation behavior of Zr_(58)Nb_3Cu_(16)Ni_(13)Al_(10) bulk metallic glass (BMG) under dry air in the glassy state and the supercooled liquid state (SLS) was studied by the thermogravimetric method. The oxidation rate and thickness growth speed in the SLS were both hugely higher than in the glassy state. The oxidation kinetics of BMG in both states for 1.5 hours was different, the parabolic law was followed in the glassy state at 300℃ and 350℃, contrarily the linear law was followed in SLS at 400 ℃. After the oxidation for 126 hours in SLS, the oxidation kinetics possessed two stages, the linear stage and the parabolic stage. The diffusion of the Cu~(2+) ion and CuZr intermetallic alloys were detected by GIXRD.
机译:通过热重法研究了Zr_(58)Nb_3Cu_(16)Ni_(13)Al_(10)大块金属玻璃(BMG)在干燥空气中的玻璃态和过冷液态(SLS)的等温氧化行为。 SLS中的氧化速率和厚度生长速度都大大高于玻璃态。两种状态下BMG的氧化动力学都不同,在1.5个小时内,在300℃和350℃下呈玻璃态时遵循抛物线律,而在400℃下SLS遵循线性律。在SLS中氧化126小时后,氧化动力学具有两个阶段,线性阶段和抛物线阶段。用GIXRD检测了Cu〜(2+)离子和CuZr金属间化合物的扩散。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号