首页> 外文会议>International conference on multi-functional materials and structures >Permanent mold Suction casting for TiAl based alloys
【24h】

Permanent mold Suction casting for TiAl based alloys

机译:TiAl基合金的永久模具吸铸

获取原文

摘要

A novel precision casting technique for TiAl based alloy was described in this work, called the permanent mold suction casting technology, and the blades of Ti-47Al-2Si、Ti-47Al-2W-0.5Si、Ti-47Al-2W-0.5Si-0.5B were get by this technology. The structures of these blades were studied. The results of this study indicate that microstructure is sensitive to heat treatment and composition. The average grain size is 30 um before heat treatment. The grain size of TiAl based alloy is grossed by heat treatment at 1573 for 5h and furnace cooling, especially Ti-47Al-2Si. The addition of boron, the grain size of Ti-47Al-2W-0.5Si-0.5B is smaller than Ti-47Al-2W-0.5Si. The γ-TiAl based alloys have equiaxed grain in cross section, but the surface microstructure of γ-Tial based alloys have more fine equiaxed grain than inside due to high cooling rate of mold.
机译:本文介绍了一种用于TiAl基合金的新型精密铸造技术,称为永久模具吸铸技术,以及Ti-47Al-2Si,Ti-47Al-2W-0.5Si,Ti-47Al-2W-0.5Si的叶片-0.5B被这项技术获得。研究了这些叶片的结构。这项研究的结果表明,微观结构对热处理和成分很敏感。热处理前的平均晶粒尺寸为30 um。 TiAl基合金的晶粒度是通过1573在5h的热处理和炉内冷却得到的,特别是Ti-47Al-2Si。添加硼后,Ti-47Al-2W-0.5Si-0.5B的晶粒尺寸小于Ti-47Al-2W-0.5Si。 γ-TiAl基合金的横截面具有等轴晶粒,但是由于模具的高冷却速率,γ-TiAl基合金的表面微观结构比内部的等轴晶粒更细。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号