SHRINKAGE OF HIGH PERFORMANCE CONCRETE

机译:收缩高性能混凝土

获取原文
获取原文并翻译 | 示例

摘要

This paper outlines an experimental and numerical study on the effect of water-binder ratio, w/b, silica fume and age on shrinkage of High Performance Concrete (HPC). Eight types of HPC were studied. Carbonation, internal relative humidity (RH) and strength were studied on cubes from the same batch of HPC that was used in the studies of shrinkage. The results indicate well correlated relationships between shrinkage, w/b and RH. The type and amount of silica fume affected shrinkage. The study was done at Lund Institute of Technology, Division of Building Materials, Lund, Sweden, in 1992-2000.
机译:本文概述了水灰比,w / b,硅粉和龄期对高性能混凝土(HPC)收缩率影响的实验和数值研究。研究了八种HPC。在用于收缩研究的同一批HPC的立方体上研究了碳化,内部相对湿度(RH)和强度。结果表明收缩率,w / b和RH之间的相关性很好。硅粉的类型和数量会影响收缩率。这项研究是在1992-2000年在瑞典隆德的隆德技术学院建筑材料部完成的。