A wet-chemical deposition method was developed to synthesize CeO_2-mica pearlescent pigment using CeO_2 as the coating material and mica as the base material. The main factors affecting the synthesis processes were studied. The optimum conditions were obtained were as: the coating reaction temperature is 70 ~ 80℃, cover ratio is 30 ~ 40%, stirring velocity is about 170 r/min, pH value is 6.50 ~ 7.50, heating rate is 3 ~ 5℃/min and heat treatment temperature is 800℃. The crystal phases and the microstructure of the pearlescent pigment powders were also analyzed by DTA-TG, XRD and SEM.
机译:开发了一种湿化学沉积法,以CeO_2为涂料,云母为基材,合成CeO_2-云母珠光颜料。研究了影响合成过程的主要因素。得到的最佳条件为:涂层反应温度为70〜80℃,覆盖率为30〜40%,搅拌速度约为170 r / min,pH值为6.50〜7.50,加热速率为3〜5℃/分钟和热处理温度为800℃。还通过DTA-TG,XRD和SEM分析了珠光颜料粉末的晶相和微观结构。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号