Consolidation and Properties of Tungsten Carbide Target with Low Cobalt Content by Hot-Press Sintering

机译:低热压烧结低钴碳化钨靶材的性能

获取原文
获取原文并翻译 | 示例

摘要

Tungsten carbide (WC) targets with low cobalt (Co) content (0.1 - 0.2 wt.%) were prepared by hot-press sintering at 1700℃ for 60 minutes in argon, from element starting powders of tungsten, cobalt and carbon. Results show that the as-fabricated targets yield relatively high relative density above 99% and high HRA above 92. WC with low Co content is formed easily than pure WC. The hot-press sintering process, while element starting powders are used, is an in-situ reaction technique for accelerating the WC's diffusion rate to obtain a dense sintered body.
机译:低钴(Co)含量(0.1-0.2 wt。%)的碳化钨(WC)靶材是由钨,钴和碳的元素起始粉末在氩气中于1700℃热压烧结60分钟而制得的。结果表明,所制造的靶材的相对密度高于99%,HRA高于92。与纯WC相比,容易形成Co含量低的WC。在使用元素起始粉末的同时,热压烧结工艺是一种原位反应技术,用于提高WC的扩散速率以获得致密的烧结体。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号