Monodispersed polymer microspheres with hydrophobic core and hydrophilic shell were prepared via a three-step method. First, polystyrene core was obtained through the emulsion polymerization. Subsequently, a relatively uniform shell containing butyl 4-vinylbenzenesulfonate was attached surrounding the core. The contents of the shell ranged from 10~40 %wt relative to that of the core. Finally, the sulfonate groups existing in the shell were converted into sulfonic acids through hydrolysis at elevated temperature, resulting in a highly charged hydrophilic shell. Infrared spectra (IR), transmission electron microscopy (TEM), differential thermal analysis, thermogravimetry (TGA) and X-ray photoelectron spectroscopy (XPS) were employed to characterize the particle structure and chemical composition.
机译:通过三步法制备具有疏水核和亲水壳的单分散聚合物微球。首先,通过乳液聚合获得聚苯乙烯核。随后,将包含4-乙烯基苯磺酸丁酯的相对均匀的壳附接在核周围。壳的含量相对于核的含量为10〜40%wt。最后,存在于壳中的磺酸盐基团通过在高温下水解而转化为磺酸,从而产生了带高电荷的亲水性壳。红外光谱(IR),透射电子显微镜(TEM),差热分析,热重分析(TGA)和X射线光电子能谱(XPS)用于表征颗粒结构和化学组成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号