A typical Fluid Catalytic Cracking Unit (FCCU) generates high temperature flue gas in the process of regenerating the catalyst. This flue gas is diverted to a stack after removal of catalyst fines and excess heat using a Waste Heat Recovery Unit (WHRU) or CO boiler. This flue gas line is a large diameter (1.2 m /2 m) piping and is a combination of Hot Wall (bare SS304H piping with external insulation) upstream of Orifice Chamber and Cold Wall (Carbon steel piping with internal refractory lining) for the downstream side. In a major revamp project, large portion of flue gas line was replaced with some dimensional and design changes. A crack was noticed at the SS304H side of hot wall to cold wall transition joint downstream of Orifice Chamber after approximately 2 years in operation. The line operates around 700 ℃ and 0.15 Bar(g) at the location of the crack. The initial crack was measured to be approximately 250 mm to 300 mm and grew to a full circumference crack in a short time resulting in minor flue gas leaking with catalyst fines. This paper discusses the details on how the issue was addressed on site and a temporary repair (i.e. welding of a box on high temperature piping) was carried out online safely, while the unit remained in operation. Further, the paper presents the root cause assessment and design modifications implemented for hot wall to cold wall transition joint during a scheduled turnaround.
机译:典型的流化催化裂化装置(FCCU)在再生催化剂的过程中会产生高温烟道气。使用废热回收装置(WHRU)或CO锅炉除去催化剂细粉和多余的热量后,该烟气被转移到烟囱中。该烟气管线为大直径(1.2 m / 2 m)管道,是孔口室上游的热壁(裸露的SS304H管道,带有外部隔热层)和下游的冷壁(碳钢管道和内部耐火衬里)的组合侧。在一个重大的改建项目中,大部分烟气管线被尺寸和设计变更所取代。运行约2年后,在孔室下游的热壁到冷壁过渡接头的SS304H侧发现了裂缝。该线的工作温度为700℃,裂纹位置为0.15 Bar(g)。测得的初始裂纹约为250毫米至300毫米,并在短时间内发展成全圆周裂纹,导致少量烟气泄漏,并带有催化剂细屑。本文讨论了有关如何现场解决该问题的详细信息,并在设备保持运行状态下安全地在线进行了临时维修(即在高温管道上焊接盒子)。此外,本文提出了在计划的周转期间从热墙到冷墙过渡缝的根本原因评估和设计修改。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号