This paper is an exploration of factors affecting internal corrosion of transmission pipeline systems (<0.5% S&W), as well as a progress report on research aimed at improving chemical mitigation of this threat in heavy oil product streams. Typical pipeline corrodents and corrodent transport mechanisms are explored.rnTransmission quality hydrocarbon products are shown to carry micro-emulsified water, various solid particles, solid particles with micro-attached water, and bacteria. While micro-emulsified water can be considered benign owing its ability to be transported harmlessly without accumulation; water-wetted solid particles have sufficient density to reach the pipe floor. Patterns of internal corrosion on a transmission pipeline are used to demonstrate the significance of solids accumulation leading to under-deposit corrosion.rnAnalysis of pipeline sludge reveals significant populations of different bacterial species indicating the existence of a robust biomass capable of creating or sustaining a corrosive environment. Corrosivity testing of pipeline sludges was performed using two static autoclave coupon methods. One test method demonstrated that the addition of chemical inhibitor directly to the pipeline sludge could reduce corrosion rates as effectively as batch treatment of a clean coupon.rnA rotating mechanical contactor was designed and built to facilitate the blending of corrosion inhibitor with pipeline sludge under 'like-pipe' flow conditions, but results of sludge corrosivity testing using this device are not yet available.
机译:本文探讨了影响输油管道系统内部腐蚀(<0.5%S&W)的因素,以及旨在改善化学减轻重油产品流中这种威胁的研究进展报告。探索了典型的管道腐蚀物和腐蚀物的传输机理。传输质量的烃类产品携带微乳化水,各种固体颗粒,带有微附着水的固体颗粒和细菌。微乳化水由于无害运输而不会积聚的能力而被认为是良性的;被水弄湿的固体颗粒具有足够的密度以达到管道底部。使用传输管道上的内部腐蚀模式来证明固体积聚导致沉积不足腐蚀的重要性。rn对管道污泥的分析表明,存在大量不同细菌物种,表明存在能够形成或维持腐蚀性环境的强大生物质。 。使用两种静态高压釜取样法对管道污泥进行腐蚀性测试。一种试验方法表明,直接向管道污泥中添加化学抑制剂可像分批处理干净的试样一样有效地降低腐蚀速率。rn设计并制造了旋转机械接触器,以促进腐蚀抑制剂与管道污泥在“相似”条件下的混合。 -管道的流动条件,但尚无法使用此设备进行污泥腐蚀性测试的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号