Low temeprautre ozone regeneration of oxoanion promoted zirconia catalysts for paraffin conversion

机译:氧阴离子促进的氧化锆催化剂的低温臭氧再生,用于石蜡转化

获取原文
获取原文并翻译 | 示例

摘要

A regeneration scheme was tried wich targeted a near isothermal operation of SO_4~2-ZrO_2 catalsyts for isomerization of n-butane; ozone regeneration at low temperature (150 deg C). A reaction-regeneration cycle in a pulse reactor was used to evaluate the properties of ozone and air for restoring the catalytic activity of the coked catalyst. Ozone was found to be able of burning the coke deposit over SO_4~-2-ZrO_2 to a great extent and an activity induction period afte rregeneration could be seen. Reaction (300degC) and regeneration (150 degC) had a temperature gap in this system. On Fe-Mn promoted O_4~_2-ZrO_2 a fully isothermal reaction-regeneration at 150 degC was hypothetically possible but O_3 treatments did not restore the doriginal activity, dur to a destructure of the promotion action of Fe-Mn onthe active sites.
机译:尝试了针对SO_4〜2-ZrO_2催化剂的近等温操作以实现正丁烷异构化的再生方案。在低温(150摄氏度)下进行臭氧再生。使用脉冲反应器中的反应-再生循环来评估臭氧和空气的性质,以恢复焦化催化剂的催化活性。发现臭氧能够在较大范围内燃烧SO_4〜-2-ZrO_2上的焦炭沉积物,并且可以看到再生后的活性诱导期。反应(300℃)和再生(150℃)在该系统中具有温差。据推测,在Fe-Mn促进的O_4〜_2-ZrO_2上,可以在150℃完全等温反应再生,但是O_3处理不能恢复原始活性,因为Fe-Mn在活性位点上的促进作用被破坏。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号