摘要

The proportion of FA - MK geopolymers mortar was proposed in terms of the results of the compressive strength. The bond tensile strength and its durability between FA - MK geopolymer mortars, which modified by polymer powder of 0, 3%, 6%, 10% dosage, and concrete slab under different curing ages and its durability of the mortars were investigated. The results indicated that the 3% dosage of polymer powder seemed to improve the bond strength slightly, and the addition of 6% and 10% water soluble polymer decreased the bond tensile strength cured at 20℃, 50%RH. The effects of the water soluble polymer of 3%~10% dosages on the bond properties are negligible at 3days curing age, the bond properties enhance with the curing age. The bond tensile strength of the mortars with 6%, 10% polymer powder reached 92%~97% of standard samples after 10 times dry and wet-freeze and thaw cycles, the bond durability can be improved remarkably. The reason is that the bend fracture energy increase with the addition of the polymer powder and the reduction of the water absorption.
机译:根据抗压强度的结果,提出了FA-MK地质聚合物砂浆的比例。研究了0、3%,6%,10%用量的聚合物粉改性的FA-MK土聚合物砂浆与混凝土板在不同固化年龄下的粘结抗拉强度及其耐久性及其耐久性。结果表明,添加3%的聚合物粉末似乎可以稍微改善粘结强度,而添加6%和10%的水溶性聚合物则降低了在20℃,50%RH条件下固化的粘结拉伸强度。 3%〜10%剂量的水溶性聚合物在固化3天时对粘结性能的影响可忽略不计,粘结性能随固化时间的增加而增强。 6%,10%聚合物粉末的砂浆经10次干湿冷冻和融化循环后,其粘结抗张强度达到标准样品的92%〜97%,粘结耐久性得以显着提高。原因是弯曲断裂能随着聚合物粉末的添加和吸水率的降低而增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号