In the Gulf of Mexico, climatic conditions with strong wind (more than 40 km/h maintained) are known as “Norths”. A “North” generates an abrupt change in the pollution level on the external insulation of power lines in a few hours. So, the pollution level is influenced strongly by climatic conditions and its behavior is very dynamic. In these conditions, the main pollutant deposited on the insulation is salt from the sea. RTV coated external insulation is frequently used in transmission lines and in substations to control pollution problems; however, the cost of this alternative for polluted areas is more expensive than the use of non ceramic insulators. Reliability for RTV coated insulators is certainly different than that for non ceramic insulators; this is the reason why some utilities prefer RTV coated insulators despite their high cost. In this work salt fog testing was done to evaluate the performance of RTV coated insulators and silicone rubber insulators during continuous conditions of high voltage and salt fog. Strings of six insulators were installed into the salt fog chamber and energized to 69 kV phase to ground, the NaCl concentration was 10 kg/m3. Insulator strings with short leakage distance either with or without RTV coating presented flashovers before 40 testing hours, while on insulator strings with large leakage distance and with RTV coating, the three flashovers developed between 400 and 500 hours. One silicone rubber insulator did not reach the flashover and the developed leakage current was lower than the measured in the coated insulator strings. It seems to be that the RTV coating is saturated with pollutant in a short time during continuous dry band arcing, consequently, hydrophobicity is lost after some hours causing flashover. The obtained results are discussed in this paper.
机译:在墨西哥湾,强风(保持超过40 km / h)的气候条件被称为“北方”。 “北部”会在几小时内在电力线的外部绝缘层上造成污染水平的突然变化。因此,污染水平受气候条件的影响很大,其行为是非常动态的。在这种情况下,沉积在绝缘层上的主要污染物是海洋中的盐分。带RTV涂层的外部绝缘层通常用于传输线和变电站中,以控制污染问题;但是,对于污染区域而言,这种替代方法的成本要比使用非陶瓷绝缘子昂贵。 RTV涂层绝缘子的可靠性肯定与非陶瓷绝缘子的可靠性不同。这就是为什么一些公用事业公司尽管成本较高但仍偏爱RTV涂层绝缘子的原因。在这项工作中,进行了盐雾测试以评估RTV涂层绝缘子和硅橡胶绝缘子在高压和盐雾连续条件下的性能。将六个绝缘子串安装到盐雾室中,并通电至与地面相接的69 kV,NaCl浓度为10 kg / m 3 。泄漏距离短的绝缘子串在有或没有RTV涂层的情况下,在40个测试小时之前都会出现闪络,而在泄漏距离大且带有RTV涂层的绝缘子串中,三个闪络发生在400至500小时之间。一种硅橡胶绝缘子没有达到闪络,并且产生的泄漏电流低于在带涂层的绝缘子串中测得的泄漏电流。在连续的干带电弧放电期间,RTV涂层似乎在短时间内被污染物浸透,因此,经过数小时后会失去疏水性,从而引起飞弧。本文讨论了获得的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号