首页> 外国专利> Purification treatment for iron composite particles of soil and groundwater that has been contaminated with organic halogen compounds, to a process for the preparation thereof, the iron purification agent comprising the composite particles, their preparation and purification treatment of soil and groundwater that has been contaminated with organic halogen compounds way

Purification treatment for iron composite particles of soil and groundwater that has been contaminated with organic halogen compounds, to a process for the preparation thereof, the iron purification agent comprising the composite particles, their preparation and purification treatment of soil and groundwater that has been contaminated with organic halogen compounds way

机译:已被有机卤素化合物污染的土壤和地下水的铁复合颗粒的净化处理及其制备方法,包括该复合颗粒的铁净化剂,它们的制备和已被有机污染物污染的土壤和地下水的净化处理有机卤素化合物的方式

摘要

PPROBLEM TO BE SOLVED: To obtain a purification agent which efficiently, continuously and economically decomposes aliphatic organic halogen compounds or aromatic organic halogen compounds included in soil or ground water. PSOLUTION: The method of producing the iron composite particle powder containing 30-99 wt.% -Fe and 3,500-10,000 ppm S for purifying soil/ground water contaminated with organic halogen compounds is to prepare iron powder particles by heating and reducing geothite powder particles having 0.05-0.50 m average longitudinal diameter and containing 2,200-6,300 ppm S or hematite powder particles having 0.05-0.50 m average longitudinal diameter and containing 2,400-7,000 ppm S at temperature of 350-600C, cool the iron powder particles, take out the iron powder particles into water without forming a surface oxide skin in the air phase and subsequently form the surface oxide skin on the surface of the iron powder particles and dry the same. PCOPYRIGHT: (C)2004,JPO
机译:

要解决的问题:获得一种净化剂,该净化剂可以有效,连续且经济地分解土壤或地下水中包含的脂肪族有机卤素化合物或芳香族有机卤素化合物。

解决方案:生产包含30-99 wt。%-Fe和3,500-10,000 ppm S的铁复合颗粒粉末以净化被有机卤素化合物污染的土壤/地下水的方法是通过加热和还原制备铁粉末颗粒。在350-600°C的温度下冷却平均粒径为0.05-0.50 m且含有2,200-6,300 ppm S的赤铁矿粉末颗粒或平均粒径为0.05-0.50 m且含有2,400-7,000 ppm S的赤铁矿粉末颗粒,将铁粉颗粒倒入水中而不在空气中形成表面氧化皮,随后在铁粉颗粒的表面上形成表面氧化皮并将其干燥。

版权:(C)2004,日本特许厅