FIELD: electricity.;SUBSTANCE: method includes electrical explosion of composite conductor exploded electrically that consists of a double-layer flat copper shell with weight of 60-360 mg and core in the form of molybdenum and graphite or technical carbon powders taken in stoichiometric ratio for synthesis of carbonaceous molybdenum with total weight equal to 0.5-2.0 of the shell weight, formation of a multiphase pulsed plasma jet out of explosion products, melting of the surface of a copper electric contact by the jet at absorbed power density of 4.5-6.5 GW/m2, deposition of the explosion products to the surface and formation of the composite coating of Mo-C-Cu system at it and subsequent repetitively-pulsed electron-beam treatment of the coating surface at absorbed power density of 40-60 J/cm2, pulse duration of 150-200 mcs and number of pulses of 10-30.;EFFECT: improved erosion-resistance of the coating.;2 ex, 2 dwg
机译:领域:电;物质:方法包括对复合导体进行电爆炸,该复合导体由重量为60-360 mg的双层扁平铜壳和以钼和石墨形式存在的核或化学计量比的工业碳粉组成用于合成总重量等于壳重量的0.5-2.0的碳质钼,由爆炸产物形成多相脉冲等离子体射流,在4.5-6.5的吸收功率密度下,射流熔化铜电触点表面GW / m 2 ,爆炸产物沉积到表面并在其上形成Mo-C-Cu系统复合涂层,随后在吸收时对涂层表面进行重复脉冲电子束处理功率密度为40-60 J / cm 2 ,脉冲持续时间为150-200 mcs,脉冲数为10-30。;效果:提高了涂层的耐蚀性。; 2 ex,2 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号