首页> 外国专利> SILICA-TITANIA COMPOSITE AEROGEL PARTICLE, METHOD FOR PRODUCING SILICA-TITANIA COMPOSITE AEROGEL PARTICLE, PHOTOCATALYST-FORMING COMPOSITION, PHOTOCATALYST AND STRUCTURE

SILICA-TITANIA COMPOSITE AEROGEL PARTICLE, METHOD FOR PRODUCING SILICA-TITANIA COMPOSITE AEROGEL PARTICLE, PHOTOCATALYST-FORMING COMPOSITION, PHOTOCATALYST AND STRUCTURE

机译:二氧化硅-二氧化钛复合气溶胶颗粒,制备二氧化硅-二氧化钛复合气溶胶颗粒的方法,形成光催化剂的组合物,光催化剂和结构

摘要

To provide a silica-titania composite aerogel particle that exhibits a high photocatalytic function in the visible range.SOLUTION: A silica-titania composite aerogel particle includes: a base particle including silicon and titanium whose element ratio Si/Ti is more than 0 and 6 or less; and a surface layer present on the base particle and including a metal compound having a metal atom and a hydrocarbon group. In a C 1s XPS spectrum, a value of [(peak intensity of C-O bond+peak intensity of C=O bond)/(peak intensity of C-C bond+peak intensity of C=C bond)] is in the range of 0.03 to 0.3. The silica-titania composite aerogel particle has a BET specific surface area in the range of 200 m/g to 1,200 m/g, and has absorption at wavelengths of 450 nm and 750 nm in a visible absorption spectrum.SELECTED DRAWING: Figure 1
机译:提供一种在可见光范围内具有高光催化功能的二氧化硅-二氧化钛复合气凝胶颗粒。解决方案:二氧化硅-二氧化钛复合气凝胶颗粒包括:硅和钛元素比Si / Ti大于0和6的基础颗粒或更少;表面层存在于基础颗粒上,并且包括具有金属原子和烃基的金属化合物。在C 1s XPS光谱中,[[(CO键的峰强度+ C = O键的峰强度)/(CC键的峰强度+ C = C键的峰强度)]的值在0.03至0.3。二氧化硅-二氧化钛复合气凝胶颗粒的BET比表面积为200 m / g至1,200 m / g,并且在可见吸收光谱中具有450 nm和750 nm波长的吸收。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号