RECLAIMING OF GROUND RUBBER TIRE BY SAFE MULTIFUNCTIONAL RUBBER ADDITIVES: III. STYRENE BUTADIENE/RECLAIMED GROUND RUBBER TIRE VULCANIZATES

机译:安全多功能橡胶添加剂替代地面橡胶轮胎:III。苯乙烯丁二烯/再生橡胶轮胎硫化

获取原文
获取原文并翻译 | 示例
           

摘要

Mechanochemically reclaimed ground rubber tire (GRT; i.e., reclaimed rubber [RR]) was revulcanized in combination with styrene–butadiene rubber (SBR). The SBR/RRblend vulcanizateswith RRcontent from20 to 80wt%were prepared and studied. Reclaiming of GRT was successfully carried out by tetra benzyl thiuram disulfide in the presence of spindle oil at around ambient temperature. The cure characteristics and physical properties of the SBR/RRblendwere studied. The optimum cure time decreased, but scorch time remain unaltered with increasing RR content in the blend. The effect of carbon black was studied in SBR/RR (80/20) blend vulcanizate to determine its ultimate use. Aging characteristics of different SBR/RR blends were evaluated.The thermogravimetric analysis, strain sweep, and dynamicmechanical analysis ofSBR/RRblend vulcanizates were examined. The thermal stability of the blend vulcanizates was decreased with an increase in RR content. Strain sweep analysis was performed to determine the RR/SBR miscibility. Temperature sweep measurement indicated that the elastic and storage modulus of the SBR/RR vulcanizates improved with increasing RR content. Scanning electron microscopy analysis was performed to study the coherency and homogeneity in the SBR/RR vulcanizate.
机译:机械化学再生的地面橡胶轮胎(GRT;即再生橡胶[RR])与丁苯橡胶(SBR)一起硫化。制备并研究了RR含量为20〜80wt%的SBR / RRblend硫化胶。在室温下,在纺锤油存在下,四苄基秋兰姆二硫化物成功地回收了GRT。研究了SBR / RRblend的固化特性和物理性能。最佳固化时间有所减少,但随着共混物中RR含量的增加,焦烧时间保持不变。在SBR / RR(80/20)混合硫化橡胶中研究了炭黑的作用,以确定其最终用途。评估了不同SBR / RR共混物的老化特性。检查了SBR / RR共混硫化橡胶的热重分析,应变扫描和动态力学分析。混合硫化橡胶的热稳定性随RR含量的增加而降低。进行应变扫描分析以确定RR / SBR的相容性。温度扫描测量表明,SBR / RR硫化橡胶的弹性模量和储能模量随RR含量的增加而提高。进行扫描电子显微镜分析以研究SBR / RR硫化橡胶中的相干性和均匀性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号