A series of spinel-structured materials have been prepared by a simple hydrothermal procedure in an aqueous medium. The new synthetic method is time and energy saving i.e., no further thermal treatment and extended grinding. The main experimental process involved the insertion of lithium into electrolytic manganese dioxide with glucose as a mild reductant in an autoclave. Both the hydrothermal temperature and the presence of glucose play the critical roles in determining the final spinel integrity. Particular electrochemical performance has also been systematically explored, and the results show that Al3+, F- co-substituted spinels have the best combination of initial capacity and capacity retention among all these samples, exhibited the initial capacity of 115 mAh/g and maintained more than 90% of the initial value at the 50th cycle. (C) 2006 Elsevier Inc. All rights reserved.
机译:通过简单的水热方法在水性介质中制备了一系列尖晶石结构的材料。新的合成方法省时省力,即无需进一步热处理和延长磨削时间。主要的实验过程涉及在高压釜中用葡萄糖作为温和的还原剂将锂插入电解二氧化锰中。在确定最终的尖晶石完整性中,水热温度和葡萄糖的存在都起着至关重要的作用。还已经系统地探索了特定的电化学性能,结果表明,在所有这些样品中,Al3 +,F-共取代的尖晶石具有初始容量和容量保持率的最佳组合,表现出115 mAh / g的初始容量,并保持了超过第50个周期的初始值的90%。 (C)2006 Elsevier Inc.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号