Atmospheric corrosion behavior of for stainless steels in contact with chlorides was studied in laboratory atmosphere. According to Shoji's method, nine droplets, each of which consist of 5 #mu#l of 0.5 N Cl~- solution, were put on a stainless steel specimen and were dried up. Thus-prepared specimens were exposed in a humidity-controlled chamber for three to six months. Penetration depth at the deposit strongly depended on RH and the maximum value of penetration depth was obtained at 50 percent RH for 430 steel and at 33 percent RH for 304 steel with the deposits of sea salt and MgCl_2, while no penetration was observed with the deposit of NaCl at 33 percent and 50 percent RH. Under RH of 75 percent all the three kinds of salt gave no penetration for 430 and 304 steels. The test was extended to seven other steels, and penetration was summarised in terms of Pitting Resistance Equivalent=(percent Cr)+3.3(percent Mo)+16(percent N).
机译:在实验室气氛中研究了与氯化物接触的不锈钢的大气腐蚀行为。 根据Shoji的方法,九个液滴,每个液滴组成5#mu#L的0.5 n Cl〜 - 溶液,被置于不锈钢样品上并干燥。 将如此制备的试样在湿度控制的室中暴露三到六个月。 在RH上强烈依赖于RH的沉积物处的穿透深度和在50%RH下获得430 rh的最大值,以33%的RH为304钢,与海盐和MgCl_2的沉积物,同时没有观察到矿床的渗透率 NaCl为33%和50%RH。 在75%的rh下,所有三种盐都没有渗透430和304钢。 该测试延伸到七个其他钢,并且在蚀性抗性等同=(百分比Cr)+ 3.3(百分比Mo)+ 16(百分比N)方面概述了渗透性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号