Si diffusion layers on SUS 310 steel surfaces were formed by halide-activated pack cementation, and their high temperature corrosion resistance was evaluated. The Si diffusion layers formed in the sample surfaces consisted of an inner layer and an outer layer. The inner layer contained 11 approx 12 mass percent Si was uniform and adhesive to the substrate metal. It was found from XRD analysis, that the inner layer consisted of two phases of alpha-Fe and Cr_3Ni_5Si_2. The thickness of the inner layer increased with an increase in the treatment time and a rise in the treatment temperature. The inner layers of 60 approx 80 mu m thickness were obtained by the treatments for more than 28.8 ks at 1223 K. The results of high temperature corrosion experiments showed that the corrosion resistance of the sample having Si diffusion layer was greatly improved by the formation of a protective inner scale consisting of SiO_2.
机译:SU 310钢表面上的Si扩散层通过卤化物活化包装胶结形成,评价其高温耐腐蚀性。 形成在样品表面中的Si扩散层由内层和外层组成。 内层含有11大约12质量%的Si是均匀的并且粘合到基材金属。 从XRD分析中发现,内层由α-Fe和Cr_3ni_5si_2的两相包括。 内层的厚度随治疗时间的增加和治疗温度的增加而增加。 通过在1223k下处理超过28.8ks的处理获得60大约80μmm厚的内层。通过形成,高温腐蚀实验的结果表明,具有Si扩散层的样品的耐腐蚀性 一种由SiO_2组成的保护性内尺度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号