A series of organosoluble polyimides with various aromatic tetracarboxylic acid dianhydrides was prepared from diamine monomers using one- and two-step methods. All the polyimides were soluble in aprotic solvents such as NMP, DMF, DMAc, and DMSO. The polyimides showed excellent thermal stability and good mechanical properties. The glass-transition temperature of the prepared polyimides ranged from 210 degrees C to 325 degrees C. All the polyimides formed tough transparent films, with tensile strength of 84- 118 MPa, 8%-12% elongation, and 1.5-2.3 GPa modulus. These polyimide films were found to have a dielectric constant in the range of 3.29-3.80 at 1 kHz and 3.14-3.76 at 10 kHz and low moisture uptake, 0.52%-1.10%. (c) 2006 Wiley Periodicals, Inc.
机译:由二胺单体使用一步法和两步法制备一系列具有各种芳族四羧酸二酐的有机可溶性聚酰亚胺。所有的聚酰亚胺都可溶于非质子传递溶剂,例如NMP,DMF,DMAc和DMSO。聚酰亚胺显示出优异的热稳定性和良好的机械性能。制备的聚酰亚胺的玻璃化转变温度为210℃至325℃。所有聚酰亚胺均形成坚韧的透明膜,拉伸强度为84-118 MPa,伸长率为8%-12%,模量为1.5-2.3 GPa。发现这些聚酰亚胺膜在1kHz下的介电常数在3.29-3.80范围内,在10kHz下的介电常数在3.14-3.76范围内,吸湿率低,为0.52%-1.10%。 (c)2006年Wiley Periodicals,Inc.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号