Single-phase ceramic samples in the morphotropic phase boundary region of the (1-y)[(1-x)(Na0.5Bi0.5)TiO3 a (TM) x(K0.5Na0.5)NbO3] a (TM) yBiFeO(3) system (N... = 0.06, 0.08, 0.10; y = 0.025, 0.05, 0.075, 0.10) have been prepared by solid-state reactions, and the effect of LiF as a low-melting-point additive (5 wt %) on the phase formation process and the dielectric properties of the solid solutions has been studied. The addition of LiF has been shown to activate the phase formation process and lower the sintering temperature of ceramic samples. The modification of the ceramics with lithium fluoride slightly increases the unit-cell parameters of the solid solutions. The addition of LiF lowers their Curie temperature.
机译:(1-y)[(1-x)(Na0.5Bi0.5)TiO3 a(TM)x(K0.5Na0.5)NbO3] a(TM)的同相相界区域中的单相陶瓷样品通过固相反应制备了yBiFeO(3)系统(N ... = 0.06,0.08,0.10; y = 0.025,0.05,0.075,0.10),并且LiF作为低熔点添加剂(已经研究了5wt%的相形成过程和固溶体的介电性能。已证明添加LiF可以激活相形成过程并降低陶瓷样品的烧结温度。用氟化锂对陶瓷进行改性会稍微增加固溶体的晶胞参数。 LiF的添加降低了它们的居里温度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号