Temperature-Dependent Shear Behavior of Geosynthetic Clay Liners

机译:土工合成粘土衬里的温度依赖性剪切行为

获取原文

摘要

The use of geosynthetic clay liners (GCLs) in barrier systems for waste containment can expose GCLs to different internal stress conditions and elevated temperatures. Thus, evaluation of the internal shear strength of GCLs as a function of normal stress and temperature is important to the design and integrity of barrier systems. In this study, internal shear strength of GCLs was evaluated in stress-controlled shear tests at a range of temperatures from 20 °C to 80 °C and under 20, 40, and 60 kPa normal stress. Horizontal shear deformation increased with increasing temperature, but decreased with increasing normal stress. Increased deformation with increasing temperature was attributed to reduced tensile strength of the needle-punched reinforcement fibers. The ratio of shear-to-normal stress at failure decreased from approximately 1.5 to 1.2 with an increase in temperature from 20°C to 80°C, and was independent of normal stress.
机译:在屏障系统中使用土工合成材料粘土衬里(GCL)进行废物围堵会使GCL暴露于不同的内部应力条件和高温下。因此,根据正应力和温度对GCL的内部剪切强度进行评估对于屏障系统的设计和完整性很重要。在这项研究中,通过在20°C至80°C的温度范围以及20、40和60 kPa正应力下的应力控制剪切试验中评估了GCL的内部剪切强度。水平剪切变形随温度的升高而增加,但随法向应力的增加而减小。随温度升高而增加的变形归因于针刺增强纤维的抗张强度降低。随着温度从20°C升高到80°C,破坏时的剪切应力与法向应力之比从大约1.5降低至1.2,并且与法向应力无关。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号