A Co based alloy powder includes between 0.08% and 0.25% mass of carbon, 0.1% mass or less of boron, between 10% and 30% mass of chromium, 5% mass or less of iron, and 30% mass or less of nickel; the iron and the nickel in a total amount of 30% mass or less; includes at least one of tungsten and molybdenum in a total amount of between 5% and 12% mass; includes at least one of titanium, zirconium, niobium, tantalum, hafnium, and vanadium in a total amount of between 0.5% mass and 2% mass; includes 0.5% mass or less of silicon, 0.5% mass or less of manganese, and between 0.003% and 0.04% mass of nitrogen; and includes cobalt and impurities as the balance of the powder. Crystal grains included in the cobalt-based alloy powder have segregated cells; the cells have an average size of between 0.15 μm and 4 μm.
机译:钴基合金粉末包括质量分数在0.08%至0.25%之间的碳、质量分数在0.1%或以下的硼、质量分数在10%至30%之间的铬、质量分数在5%或以下的铁和质量分数在30%或以下的镍;总质量不超过30%的铁和镍;包括钨和钼中的至少一种,总质量在5%到12%之间;包括钛、锆、铌、钽、铪和钒中的至少一种,总量在0.5%到2%之间;包括质量分数为0.5%或以下的硅、质量分数为0.5%或以下的锰,以及质量分数为0.003%至0.04%的氮;并包括钴和杂质作为粉末的平衡。钴基合金粉末中的晶粒具有分离的晶胞;这些细胞的平均大小在0.15μm到4μm之间。

著录项

  • 公开/公告号US11306372B2

    专利类型

  • 公开/公告日2022-04-19

    原文格式PDF

  • 申请/专利权人 MITSUBISHI POWER LTD.;

    申请/专利号US201916640207

  • 发明设计人 YUTING WANG;SHINYA IMANO;

    申请日2019-12-26

  • 分类号B22F1;C22C19/07;B22F1/05;B22F9/04;B22F9/08;

  • 国家 US

  • 入库时间 2022-08-25 00:34:22

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号