Manufacturing method of spunbonded non-woven fabric, sanitary material, and spunbonded non-woven fabric

机译:纺粘无纺布制造方法,卫生材料和纺粘无纺布

摘要

A group consisting of a propylene homopolymer having a melting point of 140 ° C. or higher, polyethylene having a density of 0.941 g / cm3 or more and 0.970 g / cm3 or less, a polymer shown in (I) below, and a polymer shown in (II) below. A fiber containing at least one polymer selected from the above, the fiber having a sea-island structure, and an island phase in a cross section orthogonal to the axial direction of the fiber, having a diameter of 0.12 μm or more and less than 0.63 μm. A spunbonded non-woven fabric having an island phase ratio of 30% or more on a number basis. (I) is a random copolymer of propylene and at least one selected from ethylene and α-olefin having 4 or more and 20 or less carbon atoms. (II) is a propylene homopolymer having a melting point of less than 120 ° C. that satisfies a specific condition.
机译:由熔点为140℃或更高的丙烯均聚物组成的组,该聚乙烯的密度为0.941g / cm 3或更高,0.970g / cm 3或更低,在下面(i)中所示的聚合物和聚合物 如下(ii)所示。 含有选自上述的至少一种聚合物的纤维,具有海岛结构的纤维,以及在纤维的轴向垂直的横截面中的岛相,其直径为0.12μm或更大且小于0.63 μm。 循环的非织造织物的岛相比为数量为30%或更高。 (i)是丙烯的随机共聚物和选自乙烯和α-烯烃的至少一种,具有4或更多和20或更小的碳原子。 (ii)是熔点的丙烯均聚物,其熔点小于120℃,其满足特定条件。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号