A nanosecond laser ablation and chemical thermal decomposition for preparing a super-hydrophobic micro-nano structure on stainless steel. The method solves the defects of long preparation cycle and complex process flow of a super-hydrophobic surface of stainless steel, and does not use fluorine-containing chemical reagents for modification. The method includes: ultrasonically cleaning a stainless steel sample piece in absolute ethanol and air-drying at room temperature; performing primary infrared nanosecond laser ablation on the sample piece to obtain a micro-nano structure; evenly coating a surface of the workpiece with micro-droplets of a stearic acid ethanol solution by using an ultrasonic atomizer; performing secondary infrared nanosecond laser ablation on the sample piece; and ultrasonically cleaning the sample piece with acetone, absolute ethanol, and deionized water respectively for 10 minutes to remove undecomposed stearic acid and slag, thereby obtaining a stainless steel super-hydrophobic surface with stable super-hydrophobic property and good quality.
机译:一种纳秒激光烧蚀和化学热分解,用于制备不锈钢超疏水微纳米结构。该方法解决了不锈钢超疏水表面的长制备循环和复杂工艺流程的缺陷,并且不使用含氟化学试剂进行改性。该方法包括:超声地清洁绝对乙醇的不锈钢样品件,室温下风干;在样品件上执行原发性红外纳秒激光消融以获得微纳米结构;通过使用超声雾化器均匀地涂覆有硬酸乙酯溶液的微液滴的工件表面;在样品件上执行二次红外纳秒激光烧蚀;分别用丙酮,绝对乙醇和去离子水清洁样品片10分钟以除去未分解的硬脂酸和炉渣,从而获得具有稳定的超级疏水性和质量稳定的不锈钢超疏水表面。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号