The present invention provides a unit quantity and water-binding material ratio (W/B) within the range that satisfies the target performance of compressive strength of 30-50 MPa to reduce cracks and vibrations of high-performance watertight concrete for ventilation using coarse aggregates. A binder for watertight concrete consisting of portland cement, blast furnace slag fine powder, fly ash, and expanded material, fine aggregate, 10~15 mm coarse aggregate, and preventing material separation while securing fluidity so that it can be obtained through a small mixing ratio It relates to a method for manufacturing watertight concrete containing a thickener and a polycarboxylic acid-based high-performance water reducing agent for Water-binder ratio (W/B) of 25-45 wt% for watertight concrete for ventilation, 150-185 Kg of water, 500-900 Kg of fine aggregate for concrete, 500-990 Kg of coarse aggregate, and thickener High-performance watertight concrete composition for ventilation for floor finishing of apartment houses that produces high-performance watertight concrete for ventilation by mixing 0.5 to 2.5% by weight of a high-performance water-reducing agent containing 2.0 to 5.0% by weight inside the portland cement It provides a manufacturing method, and provides a concrete construction method for the floor finish of the apartment house using the high-performance watertight concrete composition for soundproofing manufactured in this way.
机译:本发明提供了一种单位数量和水结合材料比(W / B),其在满足30-50MPa的压缩强度的目标性能,以减少使用粗骨料通风的高性能防水混凝土的裂缝和振动。用于防水混凝土的粘合剂,由波特兰水泥,高炉渣细粉,粉煤灰和膨胀材料,细骨料,10〜15毫米粗骨料,并防止材料分离,同时固定流动性,使其通过小混合来获得它其涉及一种制造含有增稠剂的水密混凝土的方法和基于多元羧酸的高性能降水剂的水 - 粘合剂比(W / B)为25-45wt%的水密混凝土,用于通风,150-185千克水,500-900公斤混凝土精细骨料,500-990公斤粗骨料,增稠剂高性能防水混凝土组合物,用于通风的公寓饰面,通过混合0.5生产高性能防水混凝土。 2.5%重量的高性能减水剂,含有2.0至5.0%重量的波特兰水泥,它提供了一种制造方法,并提供了混凝土用高性能防水混凝土组合物为以这种方式制造隔音的高性能防水混凝土组合物的施工方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号