METHOD FOR MANUFACTURING A PART FROM ALUMINIUM ALLOY, THE ALLOY COMPRISING AT LEAST ZIRCONIUM AND MAGNESIUM

机译:制造铝合金的一部分的方法,该合金包含至少锆和镁

摘要

The invention relates to a method for manufacturing a part comprising a formation of successive metal layers (201,....20n), superposed on one another, each layer being formed by depositing a filling metal, the filling metal being subjected to an input of energy so as to melt and to constitute the layer, by solidifying, the method being characterised in that the filling metal (15, 35) is an aluminium alloy comprising the following alloy elements, in percentages by weight: Mg: 0%-6%; Zr: 0.7%-2.5%, preferably according to a first variant >1% and <2.5%; or preferably according to a second variant 0.7-2%; or even 0.7-1.6%; or even 0.7-1.4%; or even 0.8-1.4%; or even 0.8-1.2%; at least one alloy element chosen from Fe, Cu, Mn, Ni and/or La: at least 0.1%, preferably at least 0.25%, more preferably at least 0.5% per element; impurities: <0.05% individually, and preferably <0.15% in total.
机译:本发明涉及一种制造包括彼此叠加的连续金属层(201,...... 20n)的形成的部分的方法,通过沉积填充金属来形成通过沉积填充金属来形成的每个层 通过熔化和构成层,通过固化来熔化和构成层,其特征在于填充金属(15,35)是包含以下合金元素的铝合金,其百分比重量:mg:0%-6 %; Zr:0.7%-2.5%,优选根据第一变体> 1%和<2.5%; 或优选根据第二变体0.7-2%; 甚至0.7-1.6%; 甚至0.7-1.4%; 甚至0.8-1.4%; 甚至0.8-1.2%; 至少一种选自Fe,Cu,Mn,Ni和/或La:至少0.1%,优选至少0.25%,更优选至少0.5%/元的合金元素; 杂质:<0.05%单独,总共优选<0.15%。

著录项

  • 公开/公告号EP3914748A1

    专利类型

  • 公开/公告日2021-12-01

    原文格式PDF

  • 申请/专利权人 C-TEC CONSTELLIUM TECHNOLOGY CENTER;

    申请/专利号EP20200707710

  • 发明设计人 CHEHAB BECHIR;SHAHANI RAVI;

    申请日2020-01-24

  • 分类号C22C21/06;C22C21;B22F3/105;B23K26/342;B33Y70;B33Y80;C22F1/04;C22F1/047;

  • 国家 EP

  • 入库时间 2022-08-24 22:16:57

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号