A binder solution (36) comprises greater than or equal to 0.5 wt% and less than or equal to 20 wt% of nanoparticles (36a), a thermoplastic binder (36b), and a solvent. The nanoparticles (36a) may comprise metallic nanoparticles comprising nickel, silver, chromium, aluminum, cobalt, iron, or combinations thereof. The nanoparticles (36a) may comprise ceramic nanoparticles, the comprising alumina, aluminum nitride, zirconia, titania, silica, silicon nitride, silicon carbide, boron nitride, or combinations thereof. A method (10) of manufacturing a part includes depositing a layer (22) of particulate material (24) on a working surface (32), selectively applying a binder solution (36) into the layer (22) of particulate material (24) in a pattern representative of a layer of the part, repeating the steps of depositing and selectively applying to form a plurality of layers (22) of particulate material (24) with the applied binder solution (36), and curing the applied binder solution (36) in the plurality of layers (22) of particulate material (24) with the applied binder solution (36) to evaporate the solvent and thereby form a green body part (60).
机译:粘合剂溶液(36)包含大于或等于0.5wt%且小于或等于20wt%的纳米颗粒(36a),热塑性粘合剂(36b)和溶剂。纳米颗粒(36A)可包含金属纳米颗粒,其包含镍,银,铬,铝,钴,铁或其组合。纳米颗粒(36a)可包含陶瓷纳米颗粒,包含氧化铝,氮化铝,氧化锆,二氧化钛,二氧化硅,氮化硅,碳化硅,氮化硼或其组合。制造方法的方法(10)包括在工作表面(32)上沉积颗粒材料(24)的层(22),选择性地将粘合剂溶液(36)施加到颗粒材料层(24)中的层(22)中在代表部分的一层的图案中,重复沉积的步骤和选择性地施加用施加的粘合剂溶液(36)形成颗粒材料(24)的多层(22),并固化施加的粘合剂溶液( 36)在多层颗粒材料(24)中,用施加的粘合剂溶液(36)蒸发溶剂,从而形成生坯部分(60)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号