PROBLEM TO BE SOLVED: To provide an epoxy resin-based coating composition capable of forming a coating film in which the occurrence of coating film defects such as blisters, cracks, lifting (wrinkles) and middle pus is suppressed on a coating film containing a thermoplastic resin. thing. An epoxy resin-based coating composition coated on a coating film containing a thermoplastic resin and satisfying the following (I) or (II). (I) A coating film having a dry thickness of 150 μm formed from the epoxy resin-based coating composition has a storage elasticity at 20 ° C. of 1,200 MPa or more and 6,000 MPa or less, and is an aliphatic or alicyclic diglycidyl. The epoxy resin-based coating composition containing ether (C) is an aliphatic or alicyclic diglycidyl ether (C), an amine curing agent (B), and the aliphatic or alicyclic coating composition. It contains an epoxy compound (A) other than diglycidyl ether (C), and the ratio of the content of the diglycidyl ether (C) to the content of the epoxy compound (A) is 0.4 to 1.2. [Selection diagram] None
机译:要解决的问题:提供一种能够形成涂膜的环氧树脂基涂料组合物,其中在含有热塑性塑料的涂膜上抑制了涂膜缺陷的涂膜缺陷的发生,例如泡孔,裂缝,提升(皱纹)和中间脓液树脂。事物。涂覆在含有热塑性树脂的涂膜上并满足以下(I)或(II)的环氧树脂基涂料组合物。 (I)由环氧树脂基涂料组合物形成的干厚度为150μm的涂膜在20℃下的储存弹性为1,200MPa或更高,6,000MPa或更低,并且是脂族或脂环酰基二缩水甘油基。含有乙醚(C)的环氧树脂基涂料组合物是脂族或脂环酰亚胺酰醚(C),胺固化剂(B)和脂族或脂环族涂料组合物。它含有除了二缩水甘油醚(C)之外的环氧化合物(A),与环氧化合物(A)的含量与环氧化合物(A)的含量的比例为0.4至1.2。 [选择图]无

著录项

  • 公开/公告号JP2021085013A

    专利类型

  • 公开/公告日2021-06-03

    原文格式PDF

  • 申请/专利权人 中国塗料株式会社;

    申请/专利号JP20190217032

  • 发明设计人 児玉 真尚;

    申请日2019-11-29

  • 分类号C09D163/02;C09D7/63;C09D163;B05D7/04;B05D7/24;B05D3;B05D1/36;

  • 国家 JP

  • 入库时间 2022-08-24 19:12:57

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号