Nickel-iron base alloy characterized by controlled thermal expansion coefficient and inflection temperature and by desirable high strength in age-hardened condition has composition specially restricted to overcome detrimental sensitivity to stress-concentrating geometries and aid resistance to long-enduring stress in heated oxidizing atmospheres. The alloy contains, by weight, 34% to 55.3% nickel, up to 25.2% cobalt, 1% to 2% titanium, 1.5% to 5.5% of columbium plus 1/2 the weight percent of any tantalum, up to 1% chromium, not more than 0.2% aluminum and the balance essentially iron.
机译:镍铁基合金的特征在于可控制的热膨胀系数和拐点温度,以及在时效硬化条件下具有理想的高强度,其成分受到特殊限制,以克服对应力集中几何形状的不利敏感性,并有助于抵抗在加热的氧化气氛中产生的持久应力。以重量计,该合金包含34%至55.3%的镍,至多25.2%的钴,1%至2%的钛,1.5%至5.5%的co,再加上1/2重量百分比的钽,至多1%的铬,铝含量不超过0.2%,其余部分基本上为铁。

著录项

  • 公开/公告号ATA890378A

    专利类型

  • 公开/公告日1981-11-15

    原文格式PDF

  • 申请/专利权人 HENRY WIGGIN & COMPANY LIMITED;

    申请/专利号AT19780008903

  • 发明设计人

    申请日1978-12-14

  • 分类号C22C19/03;

  • 国家 AT

  • 入库时间 2022-08-22 13:24:27

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号