PURPOSE:To efficiently briquette a powdery substance such as reduced iron to the desired size by feeding starting materials to be briquetted to a pair of flat rolls, press-molding it under excess pressure and continuously cutting the resulting molded body. CONSTITUTION:Hot powdery or granular reduced iron or prereduced ore is fed to the mixing part M of a molding apparatus 2 through a container 1 and a storage bottle 3. Pulverized coal is also fed to the mixing part M through a hopper 11, a constant feeder 12, a screw conveyor 13 and a chute 14. They are mixed in the mixing part M and fed to smooth molding rolls 5 under excess pressure applied by a screw feeder 4. A plate-shaped molded body formed by rolling with the rolls 5 is cut to a prescribed size with a pair of edged cutting rolls 6. The resulting briquettes drop into a cooling tank 8.
机译:用途:通过将待压块的原料送入一对平辊中,在过高的压力下将其压制成型,然后连续切割所得成型体,以有效地将诸如还原铁之类的粉状物质压制成所需的大小。组成:热的粉状或粒状还原铁或预还原矿石通过容器1和储藏瓶3送入成型设备2的混合部分M。煤粉也通过料斗11恒定地送入混合部分M送料器12,螺旋输送器13和溜槽14。它们在混合部分M中混合,并在由螺旋送料器4施加的过大压力下被送入光滑的模制辊5。通过与辊5滚动而形成的板状模制体。用一对切边的切割辊6将其切割成规定的尺寸。所得的团块落入冷却槽8中。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号