PURPOSE:To obtain the strength testing method after the reaction of coke characterized by high testing accuracy and high representativeness of a sample under test. CONSTITUTION:The testing accuracy can be improved by setting the particle size of a sample under test at 15mm or less and/or shortening the reaction time to less than 2 hours and more than 0.5 hour. When the amount of the sample of lump coke is set at 20kg or less, the testing accuracy can be further improved. When the range of the particle size of the sample under test us set at 3mm or more, the yield of the samples is improved, and the representativeness of the sample under test can be enhanced.
机译:目的:获得焦炭反应后强度测试方法,其特征是测试精度高,被测样品具有较高的代表性。组成:通过将被测样品的粒径设置为15mm或更小和/或将反应时间缩短至小于2小时且大于0.5小时,可以提高测试精度。通过将块状焦的试样量设定为20kg以下,可以进一步提高测试精度。通过将被测样品的粒径范围设定为3mm以上,可以提高样品的收率,并且可以提高被测样品的代表性。

著录项

  • 公开/公告号JPH04256853A

    专利类型

  • 公开/公告日1992-09-11

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CORP;

    申请/专利号JP19910018652

  • 发明设计人 NISHI TORU;ARIMA TAKASHI;

    申请日1991-02-12

  • 分类号G01N1/04;G01N1/28;G01N1/36;G01N33/22;

  • 国家 JP

  • 入库时间 2022-08-22 05:44:17

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号