PURPOSE:To improve the yield of a low boiling metal element in a molten steel with the wire addition method by setting the contact position of the low boiling metal and the molten steel at the position deeper than the bottom end of the immersion pipe of a vacuum degassing chamber. CONSTITUTION:The element having the b. p. lower than the b. p. of the molten steel 3 in the ladle 1 is coated with a metallic sheet, is made into a wire shape and is added into the molten steel. While the molten steel 3 in the ladle is returned to the vacuum degassing chamber in this method, the metallic sheet is so added as to melt in the molten steel in the region of the flow 6 of the molten steel which is discharged from the vacuum degassing chamber 2 into the ladle and flows down and the position deeper than the bottom end of the immersion pipe of the chamber 2, for example, A.
机译:目的:通过将低沸点金属与钢水的接触位置设置在比真空浸没管的底端更深的位置,从而通过焊丝添加法提高钢水中低沸点金属元素的产量除气室。组成:具有b的元素。 p。低于b。 p。钢包1中的钢水3的一部分被金属板覆盖,制成线状并被添加到钢水中。在用这种方法将钢包中的钢水3返回到真空脱气室的同时,添加金属板以使其在从真空脱气排出的钢水流6的区域中在钢水中熔化。腔室2进入钢包并向下流动,且位置比腔室2的浸没管底端深,例如A.

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号