首页> 外国专利> Chestnut - of up characteristics and resistance to hydrogen erosion characteristics superior low-alloy steel

Chestnut - of up characteristics and resistance to hydrogen erosion characteristics superior low-alloy steel

机译:板栗-优良的特性和耐氢腐蚀的特性低合金钢

摘要

PURPOSE:To manufacture a low-alloy steel excellent in creep characteristics and hydrogen attack-resisting characteristic, by incorporating specific percentages of C, Si, Mn, Cr, Mo, W, V, Al, N, P, and S to Fe. CONSTITUTION:The low-alloy steel consisting of, by weight, 0.05-0.20% C, =0.50$ Si, =1.5% Mn, 2.0-8.0% Cr, 0.1-1.6% Mo. 0.1-2.5% W, 0.05-0.50% V, =0.05% Al, =0.0050% N, =0.010% P, =0.004% S, and the balance Fe with inevitable impurities is prepared. Further, 1 or =2 kinds among 0.05-1.0% Ni, 0.005-0.08% Ti, 0.005-0.10% Nb, 0.0003-0.006% B, 0.05-1.0% Cu, and 0.005-0.06% Zr and/or either or both of 0.001-0.10% REM and 0.001-0.05% Ca can be incorporated, is necessary. In this way, the low-alloy steel suitable for use in material for pressure vessels and tubing which are to be subjected to long-period operation under high-temp. and high-pressure hydrogen can be obtained.
机译:目的:通过将特定比例的C,Si,Mn,Cr,Mo,W,V,Al,N,P和S掺入Fe中,以制造出蠕变特性和耐氢侵蚀特性优异的低合金钢。组成:低合金钢,按重量计包括0.05-0.20%C,<= 0.50 $ Si,<= 1.5%Mn,2.0-8.0%Cr,0.1-1.6%Mo.0.1-2.5%W,0.05制备了-0.50%的V,≤0.05%的Al,≤0.0050%的N,≤0.010%的P,≤0.004%的S,余量的Fe具有不可避免的杂质。此外,在0.05-1.0%的Ni,0.005-0.08%的Ti,0.005-0.10%的Nb,0.0003-0.006%的B,0.05-1.0%的Cu和0.005-0.06%的Zr和/或其中的一种或≥2种中必需同时加入0.001-0.10%REM和0.001-0.05%Ca。以此方式,低合金钢适用于压力容器和管材的材料,这些材料将在高温下长期运行。可以获得高压氢气。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号