PURPOSE: To obtain a surface frictional force enhancer compsn. capable of preventing slippage on a tile and to provide a method for enhancing the surface frictional force of the tile by forming micropores of certain size in the surface of the tile to suppress the formation of a water film on the surface of the tile. ;CONSTITUTION: This surface frictional force enhancer compsn. comprises 2-10 pts.wt. hydrofluoric acid or 3-15 pts.wt. ammonium fluoride, 1-20 pts.wt. etching relaxant and 1-20 pts.wt. dispersant. The surface of a tile is coated with a mixture of 2-40 parts of the compsn. and 60-98 pats water, allowed to stand at ordinary temp. for 3-10 min and washed with water. Micropores of about 10-900 μm size are uniformly formed in the surface of the tile, the lubricating action of a water film is inhibited and slippage is effectively prevented.;COPYRIGHT: (C)1994,JPO
机译:目的:获得表面摩擦力增强剂。能够防止在瓷砖上打滑并提供一种通过在瓷砖表面上形成一定尺寸的微孔以抑制瓷砖表面上水膜形成来增强瓷砖表面摩擦力的方法。 ;组成:该表面摩擦力增强剂。包含2-10pts.wt。氢氟酸或3-15 pts.wt.氟化铵,1-20 pts.wt.蚀刻松弛剂和1-20pts.wt。分散剂。瓷砖的表面涂有2-40重量份的混合物的混合物。和60-98拍水,使其在常温下放置。持续3-10分钟,并用水洗涤。瓷砖表面均匀形成约10-900μm大小的微孔,可抑制水膜的润滑作用并有效防止打滑。;版权所有(C)1994,JPO

著录项

  • 公开/公告号JPH06293582A

    专利类型

  • 公开/公告日1994-10-21

    原文格式PDF

  • 申请/专利权人 ANIKO:KK;

    申请/专利号JP19930081741

  • 发明设计人 RIYU SE HIYON;IMU RIYUN SON;OHAMA CHIAKI;

    申请日1993-04-08

  • 分类号C04B41/91;C09K13/06;

  • 国家 JP

  • 入库时间 2022-08-22 04:53:48

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号