Method of preparation of a sintered alloy based on iron, for a cursor of the pantograph.

机译:一种用于受电弓光标的基于铁的烧结合金的制备方法。

摘要

The sintered alloy, in order to manufacture a collector shoe on the bow to the pantograph used on an electric vehicle at high speed of 270 to 350 km / h, is prepared by mixing, as pulverulent materials which are essential, 8 to 25% by weight of elemental chromium (cr), 3 to 9% of a metal sulfide, 0,1 to 4% of boron nitride (bn), 1% or less of phosphorus (p), 3 to 8% of lead (pb) and the remainder of the iron (fe), by molding, this mixture by compression and fritting this mixture is molded in a non - oxidizing or reducing atmosphere. The ability to the compression molding can be improved by increasing the quantities of a metal sulfide and bn contained as a matter of the sintered alloy, without incorporation of lead in the substances. In this way, the lubricating power of the metal sulphide and that of the bn are used as a whole in a range of temperatures of up to 600degré c, and excellent lubricating power of the bn is used in a temperature range of 600 to 1 / p 1000degré c.
机译:为了以270至350 km / h的高速在电动汽车上使用的受电弓上制造集电弓,该烧结合金是通过将8至25%元素铬(cr)的重量,3至9%的金属硫化物,0.1至4%的氮化硼(bn),1%或更少的磷(p),3至8%的铅(pb)和其余的铁(fe)通过模压成型,通过压缩和熔结将该混合物模制在非氧化或还原气氛中。通过增加作为烧结合金的金属硫化物和bn的含量而没有在物质中掺入铅,可以提高压缩模塑的能力。这样,在高达600℃的温度范围内整体使用了金属硫化物和bn的润滑能力,在600至<1的温度范围内使用了bn的优良润滑能力。 / p 1000度

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号