Procedure for obtaining soft flexible polyurethane foams with viscoelastic and damping properties of sound and mixtures corporeo polyoxyalkylene polyol used for this purpose.

机译:获得具有声音的粘弹性和阻尼特性的软质软质聚氨酯泡沫的方法以及为此目的所用的可混合的聚氧化亚烷基多元醇多元醇。

摘要

INVENTION: PROCEDURE INVOLVES A; WHAT TO PRODUCE FOAM soft and flexible polyurethane employed with viscoelastic properties AND SOUND ABSORBING at a temperature between -20 and 80 CY MIXER comprises treating polyoxyalkylene polyol-modified organic polyisocyanates in the presence of catalysts, solvents ( WATER), AUXILIARY SUBSTANCES AND ADDITIVES USUAL AND DESCRIBE MIXTURES polyoxyalkylene polyol containing a mixture BLOCK polyoxypropylene-POLIETILENO polyol have a number of HIDROXI 14 TO 65 AND CONTENT ethylene oxide units 2 to 9% by weight relative to the weight of the polyoxypropylene units and are obtained by polymerizing 1,2-propylene oxide anion with a functionality of 2.3 to 2.8, at elevated temperature and in presence of water, glycerol and / O trimethylolpropane and polymerization of ethylene oxide in the adduct polyoxypropylene.
机译:发明:程序涉及A;生产泡沫的方法具有柔软弹性和柔韧性的聚氨酯,具有粘弹性和在-20至80 CY的温度之间吸声。MIXER包括在催化剂,溶剂(水),助剂和添加剂存在下处理聚氧化烯多元醇改性的有机多异氰酸酯。描述混合物包含嵌段聚氧化丙烯-POLIETILENO多元醇的混合物的聚氧化烯多元醇具有HIDROXI 14至65的数量和相对于聚氧化丙烯单元的重量为2至9重量%的环氧乙烷单元,并且是通过聚合1,2-环氧丙烷而获得的。在升高的温度下,在水,甘油和/ O三羟甲基丙烷的存在下,官能度为2.3至2.8的阴离子和加合物聚氧化丙烯中环氧乙烷的聚合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号