FIELD: adhesive compositions. SUBSTANCE: the invention makes it possible to improve the procedure of applying a composition, improve adhesion strength up to 0.15-0.18 kH/m and improve light resistance of the glue seam up to 9 or 10 days. The composition comprises (wt %): 8.0-12.0 polychloroprene rubber; 1.8-3.4 indenecoumarone resin; 0.79-1.57 a filler; 0.3-2.2 melamine-formaldehyde resin; 0.4-1.4 alkyd resin; and a solvent, the balance. The composition is prepared by rolling the composition on cooling rolls for 5 to 10 minutes, adding magnesium oxide and rolling for another 5 to 10 minutes, adding zinc oxide, rolling for another 5 minutes, taking the rubber off the rolls, cutting it through and feeding it into an adhesive agitator together with toluene or ethyl acetate. After the rubber has fully swollen, indene-coumarone resin, melamine-formaldehyde and alkyd resins or varnish based thereon are added and a third portion of the calculated amount of methylene chloride is introduced. After the mixture becomes homogeneous, the remaining part of methylene chloride is added and the whole is stirred for 20 to 30 minutes. EFFECT: improved properties of the adhesive composition. 1 tbl
机译:领域:粘合剂组合物。物质:本发明使得可以改善施加组合物的步骤,将粘合强度提高至0.15-0.18 kH / m,并且将胶缝的耐光性提高至9或10天。该组合物包含(重量%):8.0-12.0的聚氯丁二烯橡胶;和1.8-3.4茚并香豆素树脂; 0.79-1.57填料; 0.3-2.2三聚氰胺-甲醛树脂; 0.4-1.4醇酸树脂;还有一种溶剂,即余额。通过将组合物在冷却辊上滚动5至10分钟,添加氧化镁并再滚动5至10分钟,添加氧化锌,再滚动5分钟,将橡胶从辊上取下,切下并通过该组合物来制备该组合物。将其与甲苯或乙酸乙酯一起送入粘合剂搅拌器中。在橡胶完全溶胀之后,加入茚-香豆酮树脂,三聚氰胺-甲醛和醇酸树脂或基于其的清漆,并引入计算量的二氯甲烷的第三部分。混合物变得均匀后,加入剩余的二氯甲烷,并将其整体搅拌20至30分钟。效果:改进了粘合剂组合物的性能。 1汤匙

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号