FIELD OF THE INVENTION The present invention relates to a method and apparatus for the treatment of natural calcareous fibrate or compound based, pulverulent base material for the preparation of a hydroulphite binder consisting of a stable mixture of α-anhydrite and bassanite, wherein the? Further, the present invention relates to a hydrocyanic binder based on calcium sulfate. The essence of the process is the following consecutive steps of heat-stone mining. (a) heating the spongy material to a temperature substantially between 220 ° C and 360 ° C in the presence of water vapor, under conditions which are suitable for producing mainly calcareous feldspar, (b) subjecting the material so heated to a temperature of at least 150 ° C; In less than 15 minutes with the help of cold, dry gas injected into the material under pressure. The essence of the apparatus comprises a heat-burning tunnel (1), in which heat-sinking troughs (5) are placed adjacent to one another and the troughs (5) are provided with means (8, 9) to heat the vibrations, furthermore and below the tunnel (1) there is a cooling device (2) having a heat-shrinkable container (17) and a means (20) for heating it to vibration vibration, further the material is gravitated from the lower end of the tunnel (1) a cooling means (26) comprising cold means for injecting cold compressed air (21, 22, 23) and means (24, 25) for removing material from the lower end of the cooling device (2). The essence of the hydrocyclic binder, heat, is a stable mixture of α-anhydrite and bassanite in which the weight ratio of α-anhydrite is greater than 35%. ŕ
机译:天然钙质纤维状或化合物基粉状基质的制备方法和设备技术领域本发明涉及一种用于处理天然钙质纤维状或化合物基粉状基质的方法和设备,该粉状基质材料用于制备由α-无水石膏和重钙铝石的稳定混合物组成的水合亚硫酸盐粘合剂。此外,本发明涉及基于硫酸钙的氢氰酸粘合剂。该过程的实质是热石开采的以下连续步骤。 (a)在适用于主要生产钙质长石的条件下,在水蒸气存在下,将海绵状材料加热至实质上介于220°C至360°C之间的温度,(b)使如此加热的材料于0至少150°C在不到15分钟的时间内,借助冷的干燥气体在压力下将其注入材料中。该设备的本质包括一个热通道(1),其中散热槽(5)彼此相邻放置,并且该槽(5)设有加热振动的装置(8、9),另外,在隧道(1)的下方,有一个冷却装置(2),该装置具有一个可热收缩的容器(17)和一个将其加热至振动的装置(20),另外,物料从隧道的下端被引出。 (1)冷却装置(26),包括用于注入冷的压缩空气(21、22、23)的冷装置和用于从冷却装置(2)的下端去除材料的装置(24、25)。水环粘合剂的本质是热量,是α-硬石膏和重钙铝石的稳定混合物,其中α-硬石膏的重量比大于35%。 ŕ

著录项

  • 公开/公告号HU9802919A2

    专利类型

  • 公开/公告日1999-03-29

    原文格式PDF

  • 申请/专利权人 ENERGETIC INDUSTRIES INTERNATIONAL S.A.;

    申请/专利号HU19980002919

  • 发明设计人 DUSSELCHRISTIAN;

    申请日1996-04-24

  • 分类号C04B11/05;C04B11/028;F27B9/24;C04B28/16;

  • 国家 HU

  • 入库时间 2022-08-22 02:27:16

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号