FIELD: tube production. SUBSTANCE: method comprises steps of forging ingot to rod at several transitions and at temperature of α-range in transitions from first until last but one and at temperature of (α+β)-range in last transition; cutting rod by lengths of multiple value, drilling axial hole in it, extruding intermediate billet at normalized ratio of temperature and elongation values, cutting received blank by lengths of multiple value, boring axial opening, turning lateral surface and finally extruding billet at normalized ratio of temperature and elongation values. Temperature and elongation values at intermediate and final extrusion processes are calculated according to claimed formulae. EFFECT: finely dispersed uniform microstructure along thickness of tube wall. 1 cl
机译:领域:管材生产。物质:该方法包括以下步骤:在多个转变处以及在从最初到最后的转变中在α范围的温度处锻造锭料,而在最后一个转变中以(α+β)范围的温度进行锻造。以多值长度切割棒,在轴上钻孔,以标准化的温度和伸长率比率挤压中间坯料,以多值长度切割接收坯料,钻孔轴向开孔,转动侧面,最后以标准比率挤压坯料温度和伸长率值。根据要求保护的公式计算中间和最终挤出过程中的温度和伸长率值。效果:沿着管壁的厚度细微分散均匀的微观结构。 1厘升

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号